Seeking technology for silver plating aluminum  

+

I need technology for silver coating Aluminum.

Goran
Lavica Komerc - Belgrade, Yugoslavia


+

I DIDN'T KNOW CLEARLY WHAT YOU MEAN BY COATING BUT IF YOU MEAN ELECTROPLATING THEN I THINK THIS PROCEDURE WILL HELP

1-CLEAN THE SURFACE OF ALUMINIUM

2-ETCHED IT WITH [SODIUM HYDROXID]

3-IMMERSE IT IN ZINCATING SOLUTION

4-REMOVE ZINCATING BY NITREC ACID

5-ZINCATING AGAIN

6-ELECTROLESS NICKEL

7-ACIDIC COPPER

8-NICKEL

9-SILVER PLATING

RAFAAT ALBENDARY
NATIONAL PLASTIC ELECTROPLATING - CAIRO, EGYPT


Dear Reader, please --
Post a question on a different subject.
 
Answer or follow-up on this subject (in non-commercial fashion).
 

 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com