Gauge to check uncured powder thickness?

+

Is their a mil gage to check uncured powder?

Jerry [last name deleted for privacy by Editor]
- Grand Rapids, Michigan


+

Yes there is a device available to measure the film thickness of un-cured powder coating. The process involves laser technology and is quite expensive, and can only measure at one given height.

Hope this helps.

Drew Devlin
- North Lincolnshire, U.K.


March 10, 2009

Gauges are available to measure the uncured powder. The gauges uses ultrasonic technology to measure uncured powder coatings without contacting the surface and predict the final thickness of the coating after cure.

Chris Beninati
- Rochester Hills, Michigan


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search