Letter 8039

Acid copper with higher thickness 

+

My acid copper plating plant can't do 200 to 250 microns plating. It takes too much time to do high thickness plating. Plating also pilling after getting thickness. Have you any process to get thickness speedily without pilling?

Vinay Talsania