Seeking Chrome-6-free Zinc Cobalt Plating Service
+
We require a plating process to exceed 480 hours salt spray following a 160 degree centigrade bake for 2 hours. However this process must not contain Chrome 6.
One solution offered by a company in France was Zinc Cobalt but I have not been able to find a contractor in the UK to plate these steel components.
Any suggestions on contractors for Zinc Cobalt or alternative plating that conforms to BMW's "Black" list (prohibited substances)
Mr. Jones- UK
+
Dear Mr Jones,
The way to meet the spec is to use Zinc- iron with a triavalent Black Chromate. I have word from Surtec Gmbh, that they have a Triavalent Black Chromate available.
rgds,
|
Khozema Vahanwala Saify Ind Bangalore, Karnataka, India |
|