I want to import some sinuous wire 1070 tensel strength 1/4 rod. I
want to find out how to process to give a clean, shiny appearance
that will not rust for 6 mos-one year.
Noland
- Chino, CA, USA
+
Is this rod made of steel? I will assume that it is. You may want
to try galvanizing or zinc electroplating. For a very nice looking
appearance, you can look at nickel plating (electroplating or
electroless). Nickel will probably be expensive, but it depends on
what your requirements for appearance are.

Tim Neveau
- Rochester Hills, MI