You will get better support from this site if you make your questions specific instead of general. BOOKS have been written on the subject of electroless plating of copper and nickel, and we don't have time here to do what you need. However, there are many suppliers out there who want to sell you electroless copper and/or nickel; why don't you contact them?

James Totter, CEF
- Tallahassee, Florida


+

CuSo4=15g/l
rochel salt60g/l
NaOH=35g/l
formaldhid=20g/l
NiSO4=0.5g/l

I think I help u in your work.

With my best regardless,

Maher
G.L.S. - Cairo, Egypt


Dear Reader, please --

Post a question on a different subject.
 
Answer this question (in non-commercial fashion).
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com