Aluminum in Zincate bath
+
Does anyone know if there is a way to remove the aluminum from a zincate solution?
Abgie Molnar
- Fort Saskatchewan
+
Abgie,
I would try with electrolysis, because exchange resins keep both Aluminium and Zinc. I found this site: www.tinaja.com/glib/muse114.pdf
Good luck and let me know
Francesco Cicchetti
- Sulmona, Italy