Abrasion test (hardness test) for SnPb plating
+
Looking for abrasion test (hardness test) for SnPb plating thickness 10 micron. Any idea?
Norbert Pielmeier
- Richmond, VA, USA
+
Look up "Taber Abraser" testing and see if there is a protocol suitable for your needs.
|

Ted Mooney, P.E.