letter 7078
Plating on Tellurium
Copper
+
Are there any suggestions to plating on Tellurium Copper? We have
tried a variety of acids/dips (fluoboric included), peroxide and
other processes, only to get a very "grainy" deposit. Sometimes we
have peeling as well and have tried an acid copper, but have also had
limited success. Most of the tellurium that we are getting in
requires silver or gold plating. We have seen a rise in Tellurium of
late, which I am sure is due to the Beryllium Copper shortage. Any
suggestions would be greatly appreciated!
Jeff Smith
- Franklin, IN USA
Dear Reader, please --
- Post a
question on a different subject.
-
- Answer this question (in non-commercial
fashion).
-
 |