Corrosion of metals by iode/iodine solution 

+

I am looking for a metal resistant to the corrosion by a iode/iodine (I2/I-)solution. This is for application in dye-sensitised solar cells.

Pedro EnrÌquez Fernandez
Fundacion centro nacional del vidrio - La granja (Segovia) SPAIN


+

Nickel resists iodine well, but not sure about other iodine compounds, nor alloys such as stainless steel that contain nickel. Vanadium is also rated good, but stay away from tantalum and molybdenum. I would consult with a commercial source for these exotic metals, and also check if a plating, or other surface coating methods, applied to a less expensive substrate would work.

W. Carl Erickson
- Rome, New York


Dear Reader, please --
Post a question on a different subject.
 
Answer this question (in non-commercial fashion).
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com