Letter 7037

Wipe on silver replating  

+

Several years ago I was able to purchase a product called "The Silver Solution" from one of our upscale department stores. It was a wipe/rub on type of silver replating. The item came in a kit that also included a special silver cleaner. It did a wonderful job of maintaining and covering small worn spots on vintage/antique silver plate items. I am no longer able to find this product and am hoping there is another product similar to this available. My question is whether or not you know of any product currently available and where it may be purchased? I think this would be useful information to anyone with silver plated items that need to be touched up. Thank you!

Wendy Isaacson
- King, NC USA


+++

Found the link to The Silver Solution. Do not have any personal experience with the product myself as of yet.

Mike Palladino
- Highland, NY

----
Ed. note: Wendy -- some alternatives are Jax Silver Plating Solution, Medallion Liquid Silver Plating Solution, Miracle Silver, Nu Silver, Quickshine, Silveron, Silver Plating Formula, and Silver Secret. We've added an
FAQ page that sources those products.

Mike -- thanks for the link. We've moved it to the FAQ page because it was proving impossible to keep links current when scattered across dozens of different letters on the same subject.


May 1, 2008

I used Miracle silver plus it is the best product out on the market they bought nu silver if you need to see a great product try that it is awesome.

jeff galpern
- Boca Raton florida USA

----
Ed. note: Glad you found something you like, Jeff; but with the anonymity of the internet, superlatives can start a race to the bottom. Maybe we should just leave it that you think it's a good product rather than that every other product is inferior to it:-)

 


June 15, 2008

You might also try Medallion Liquid Silver. As a retired antique dealer I have used this item many times and love it. That's why I sell it.

Sue Rosendall
- Venus, FL, USA


Dear Reader: please choose what you want to do.

I want to post a question on a different subject.
 
I want to answer this question publicly.





 

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com