Letter 7034

Seeking rhodium plating chemicals

+

Where can I get chemicals Rhodium electro-plating. Please help. I am just hobby person. I will plate some momentos and small medical instruments

Thanks, sincerely,

Rajendra K. Bhama, M.D.
- Canton, MI, USA


+

Rhodium plating may be done by two ways.

1) Rhodium pen plating.
2) Rhodium dip (bath) plating.

You can more information about both these processes, equipments and supplies from the following companies.

Red sky Plating
Technic Inc.

Hope this information helps you.

Thanks

ajit

Ajit Menon
United Precious Metals Refining, Inc. - Alden, New York


Dear Reader, please --

Post a question on a different subject.
 
Answer this question (in non-commercial fashion).
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com