My company is called Toly Products and we are an injection moulder
of plastics packaging for the cosmetic industry based in
London,England. We have a need to find a company based in England who
is capable of white brass electroplating onto ABS Plastic mouldings
which we produce.The mouldings are approx 100mm dia and look a bit
like a very small car hubcap which has a radius of approx 200mm. Is
it possible that you know anyone who can help or an association like
yours here in the UK that we can approach.
DAVID THOMAS
- Wembley London England
+
Sir:
All I can say is "WOW." It has been over 20 years since I have
heard of white brass being offered on the open market. It was offered
during a nickel shortage, for application on parts in lieu of nickel
plating. As I recall it even used specially made alloy anodes of Zinc
and a small amount of Copper.
The manufacturer of the process was DuPont, but they have been out
of that market for decades. I suggest that you scan the plating
process suppliers in the U.K., first to see who might even still make
this. Then, you may find someone who is using it.
Sincerely,
Ed Budman
 
Ed Budman