Copper roof aging unevenly

.

We have a copper roof over our bay window. It is about 15 years old. The front half of the roof is green, while the rear half is brown/red tones. Over the years, when water has spilled out from the second story gutter above, it has caused the roof to discolor and age unevenly.

Is there any way to even out the color to be either green or brown/red?

Is it possible to "seal" the copper roof so this doesn't happen again over time?

Tracy S [last name deleted for privacy by Editor]
- Kernersville, North Carolina


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search