Hours of salt spray for electrogalvanized auto body

     

.

Dear sir/madam

At the moment I am trying to find out what is the recommended hours for salt spray test for auto body zinc coated (electrogalvanized) panel sheet to SAE and ASTM standard. thank you for answering.

regards

Nariman

Nariman Mirzade zare
- Tehran, Iran


.

Specific pass/fail requirements for corrosion are nearly always specified by OEM specifications and not by SAE or ASTM specs. You will have better luck looking for a specific automotive company's spec for auto bodies. Corrosion specifications differ from one component to another, which is why there is usually not a generic spec.

Tim Neveau
Rochester Hills, Michigan

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search