Letter 6068

Seeking custom-made titanium anodes for chlorinators [Australia]

.

We recently found you on the internet and would like to know if you can manufacture anode material for use in salt water chlorinators.

We have been manufacturing chlorination equipment for over 25 years, and use various types of anode, namely:

1. 15,000 hour titanium plate and mesh coated with ruthenium/iridium
size: 1mm x 1000 x 305 mm or greater (1005 x 1030 mm)
current density: approximately 520 amps/sq.m
Operating temperature: 15*C - 35*C
Water salinity (NaCl): 0.5% salt

2. 45,000 hours anode - used for commercial applications. All in solid plate coated titanium
size: as in paragraph 1 except no mesh only plate, 1.5 mm & 1mm. thick
current density: approximately 520 amps/sq.m
Operating temperature: 15*C - 35*C
Water salinity (NaCl): 0.5% salt

3. Reverse Polarity Anodes. All Plate
size: same as in paragraph 1 except all plate (1mm. thick)
current density: 320 amps/sq.m (approximately)
Operating temperature: 15*C - 35*C
Water salinity (NaCl): 0.5% salt
Reversing frequency: every 12 or 24 hours (this can be varied)
Life: approximately 10,000 hours.

Kind Regards

Kerry Gosse, Managing Director
Australia


Dear Reader: there is no provision for public reply to this particular letter because it is a commercial inquiry to which our advertisers will reply in private --

I want to post a question or inquiry of my own.
 
I am a supporting advertiser and want to reach the inquirer privately.

 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com