SURFACE DEFECTS ON HOT DIP GALVANIZED STEEL SHEET

.

Dears,

I am a working as a quality control Inspector in Pakistan Steel for 17 years and I want to improve my technical knowledge & skills about surface defects on hot-dip galvanized steel sheet.

Please send me details about surface defects with pictures and their causes on hot-dip galvanized steel sheet.

I will be very thankful to you if you will send me details about surface defects of hot-dip galvanizing.

Ayub Naqvi
steel - Karachi, PAKISTAN


+

Hello,

You can find related information in the book Faults in Hot Dip Galvanizing [link is to info about book on Amazon] by Dietrich Horstmann Verlag 1983 Stahleisen MBH Dusseldorf Germany.

Oktay Elkoca
iron and steel works - Kdz. Eregli, Zonguldak, Turkey


+

I would to know any informations about optimalizations of quality hot dip galvanized steels for automobily industry

Peter Sucka
- Kosice - Slovakia


++++++

I would like to have pictures of quality defects of a flat product hot dip galvanized steel.

Sami Ali
steel manufacturing - Saudi Arabia


April 20, 2008

Dear Friends

If you need more information about hot-dip galvanizing, including its properties, defects and optimization, you can go to:
http://www.teckcominco.com/Generic.aspx?PAGE=Products+%26+Services+Pages%2fTechnical+Library&portalName;=tc

Hamed Asgari
Isfahan University of Technology,Steel Institute - Isfahan, Iran


April 15, 2010

Why white patch marks is coming in my hot dip galvanizing process

Manas Mukherjee
Quality Head - Patna, Bihar, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search