Letter 6010 Anodize. I'm looking for a liquid that can be applied then rinsed or wiped off, to be baked to 150 c ,later in the process. Is there such a liquid? Bob N
. Yes.... I mean no....I mean....What was the question again?
. errr....huh? Ditto to your answer, Ted..sorry, I couldn't resist.
OKAY, OKAY, YOU JOKERS, the answer is "What are you trying to accomplish with this liquid?" It is not anodize, it might be a chromate conversion coating, which can be applied to aluminum with a brush or a rag. Baking to 150C might be a bit too high to preserve the corrosion protection properties of a conversion coating.
May 23, 2006 Hey ! is there anyone know what chemical can make the aluminium
surface bright and shining Ong Lip Khoon
May 29, 2007 If you've seen bright and shiny parts like that. Ong, they were probably bright and shiny BEFORE anodizing, not made bright after it.