Can anyone advice what is the process, chemical use to coat/plate the surface of the stainless steel matte black? Does this process adhere to certain forms of standards?

Thank-you

Regards
Hong

HN Hong
product designer - Singapore
  ^- Privately contact this inquirer -^
November 20, 2009

Hi, Hong. Electroplating with black chrome, black nickel, or black zinc might do what you wish. Black nickel would probably be easiest for stainless steel.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


January 13, 2010

You could also anodize the stainless.

Robert H Kinner
- Toledo, Ohio


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search