Deburring Titanium
November 9, 2009
Can I remove the edge/corner of titanium parts with tumbling or vibrating media?
I want to get a .005" to .010" radius on the edges.
What Type/size media (i.e. ceramic) do you recommend?
Aerospace - Hampton, VA, USA
^- Privately contact this inquirer -^
November 10, 2009
Yes.
What is the size of your parts.
The larger the media the faster it will work.
|
AF Kenton Huntingdon Valley, Pennsylvania |