Is it Industry Standard to passivate 316L
Stainless Steel after welding? [Washington]
October 24, 2009
Working on a project using 316L steel metal, advised fabricator
that passivation of the welds should be done. For whatever reason
they were not done in the shop and now the question arises "you never
provided written direction to passivate" ?
John Koch
specifier - LaConner, WA

October 31, 2009
John,
Your fabricator is right,if you did not ad it to the written specs,
he does not have to passivate.
It is not industrial standard to passivate SS. Following the written
specs is industrial standard.
But he will certainly do it if you order it and accept the additional
cost.
Kind regards,
Marc.
Marc Quaghebeur
- Diksmuide, Belgium, Europe
-
-
 |