Appearance of #4 finish on stainless vs aluminum
October 13, 2009
I need to figure out if a #4 finish looks the same on Aluminum as it does on Stainless..any thoughts. My guess is that it doesn't look as reflective on Aluminum?
Thanks
metal worker - Oakland, California
^- Privately contact this inquirer -^
October 16, 2009
Hmmm. Technically speaking, they should be nearly identical in smoothness. Appearance will be different because of the metals.
|