What kind of stainless steel is resistant to 93% sulphuric acid? [Finland] 

October 13, 2009

Good day! What kind of stainless steel resistant to sulfuric acid 93%?
(I need hose fittings for sulfuric acid 93%transportation)
Maybe AISI 316Ti?
Thanks,

Jerry Fox
engineer - Finland
contact button


October 29, 2009

Better go for SS 316L

Kannan B
- Salem,Tamil Nadu,India