We make a fine mixture of White cement + plaster of paris +
general purpose adhesive( Fevicol) + water in thick form. We have
aluminium plates having 4 portions of 12 mm wide and 12 mm deep. We
fill it with mixture and put our small articles in between it and
align it properly. Then we baking it in an electric oven for quick
drying and no more shrinkage which could unalign our articles.
After our process is complete we remove our article.
Now we are facing problem to remove the dry mixture. It is not at all
easy. Is there any solution to remove it fast?
Bankim Bhatt
Buyer - Ahmedabad, Gujarat, India

October 8, 2009
Hi, Bankim. If the plates were coated with Teflon impregnated
electroless nickel plating, I think there would be greatly reduced
sticking.