Hi
We are a company in Sweden that works with stainless steel and we have a problem.
After we welded together two sheets grinded stainless sheets grit 220 we need to grind down weld and restore welded area so it blends in with grinded area. Because sheets are big we don´t want to grind and polish whole sheets with scotschbrite. Today we use a linear grinding machine PTX 300 from Eisenblaetter but it takes too long time.

Hope You can help us with this problem


Best Regards

Fredrik Björn
salesman - Växjö, Sweden
contact button


October 2, 2009

Long is a relative term. Reworking/ blending in welds is probably one of the most difficult aspect of surface finishing and there aren't many short cuts other than automation. There are some chemical processes that can be used to restore a uniform surface, but it won't blend in uneven surfaces.

AF Kenton
Nova Finishing Systems Inc.

Huntingdon Valley, PA


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com