53099
Need Gold Plating of Silver Chalices
[Florida]
September 15, 2009
Need 24 chalices to be gold plated, original gold came off with
very little use. Only the inside of the cup needs to be plated and
only the bottom half of the cup lost the gold. The cups measure about
3" in diameter and about 3" deep.
James Kurps