53096
Stainless steel tank coating
[Texas]
September 14, 2009
I made a submersion tank for some heat exchaners out of 304
stainless.The tanks started to rust a wee bit after a leak check.Is
there a coating I can put on it to prevent it from doing this?
Thanks!!
Bryan
Bryan Bagnell
machinist - Dallas, Texas, USA

September 16, 2009
Really not enough information for a good answer. You could grit
blast it clean and coat it with a liquid PVC or a liquid vinyl or you
could put a vinyl or plastic liner in it or you could fiberglass it
or??
James Watts
- FL
-
-
 |