53077

Need Dacromet (black) on SAE 1050 spring steel components [Virginia] 

September 11, 2009

Fuel Injector clip coating needed to handle 500 hrs of Salt Spray Testing current recommendation are a Black Dacromet coating. The material being coated is SAE 1050 spring steel heat treated to 70-77

Ryan Loer
recreational vehicle fuel systems - Newport News, Virginia