Need CARC painting shop /service
I am looking for a carc finish (black) This is a government contract. Please see specs.
Clean spec. TT-C-490
Treat type I or III, Spec TT-C-490
Prime Spec Mil-P-S2192
Mil-P- 53030 or Mil-P-53022
Finish Coat- Black
Film thickness to be in accordance with MIL-STD-193
parts 1.) Door Hinge Assy. Weight per piece 8.6oz 20,000 pc's This is ongoing and there is additional parts with same spec.
a mfgr, of stampings, forgings and wire forms in Bristol, Connecticut, USA
^- Sorry! This RFQ is outdated -^
+++++++
Small N.E. company seeks to partner with a paint shop that is familiar with CARC painting. Pricing must be competitive - this isn't a $100 hammer opportunity! We're looking for someone who wants to make a profit not a killing. 5 parts = 1 kit. Production of 34 kits/wk at maximum production.
R.S. H. [last name deleted for privacy by Editor]Composite Manufacture - Bennington, Vermont, USA
^- Sorry! This RFQ is outdated -^
+++++++
Need to find CARC painters in the CT - NY - NJ area for a high volume job (2,200 parts per month - parts weight approx. 110 pounds).
Work will begin IMMEDIATELY. If you have the capability to do CARC painting please contact me at the e-mail address and I will have one of our reps contact you.
Fabrication - Avon, Connecticut, USA
^- Sorry! This RFQ is outdated -^
+++++++
Need to find CARC ( MIL-C-53039A sand color # 33303) painter in San Diego CA area for small castings (largest is 12 in x 8 in x 4 in deep) and small aluminum parts. Service require to do some masking also. This will be an on going program (approx. 100 parts per month) with great potential of expansion.
Marco P. [last name deleted for privacy by Editor]Mfg Engineer - San Diego, California, USA
^- Sorry! This RFQ is outdated -^
+++++++
LOOKING FOR A COMPANY TO DO MILITARY PAINTING (MID-WEST AREA)
CARC PAINTING IN ACCORDANCE WITH 12369001,12369002, ETC.
FOR LARGE QTY ORDERS WITH REASONABLE PRICES 15,000 - 60,000 PARTS ON DIFFERENT QTY ORDERS on small parts send info by email
thanks,
MACHINE SHOP - PUEBLO, COLORADO, USA
^- Sorry! This RFQ is outdated -^
June 16, 2009
Finishing.com:
I need to locate painting vendors to support a large CARC
(Mil-DTL-64159 Waterborne Chemical Agent Resistant Coating) requirement. They need to be located within 250 of Charlotte North Carolina.
The following finishing description is typical as required by vendors.
Finishing Process Elements/Steps:
-Pre-Wash
-Water Break Test (ref: Surface Cleanliness)
-Sand Blast Per NAC 3 Classification (Near White)
-Pre-Paint Preparation (mask, plug, etc.)
-Prime
-Final Coat
Note: Basic Facility Requirements to include ISO: 9000:2001, CARC Certification or Compliant
Please advise if you know of any suppliers, or can point me to a web site or organization that can assist to identify.
Thank you,
mfg for Mil-Spec fabrications - Charlotte, North Carolina, USA
^- Privately contact this inquirer -^
August 14, 2009
I have a part that is approximately 110 pounds that I need primered and CARC painted. Current need is 200 pieces. If things go well we have projects that require priming and CARCing from time to time