Need Coating/Paint that looks like Clear Anodized Aluminum [California] 

July 13, 2009

We use cast aluminum parts of mixed/unknown alloy aluminum. Our usual vendors have been unable to give them a good-looking anodized finish because of the impurities/porosity in the metal. We want them to look "frosty" like our other, machined parts which anodize quite well because they are alloy 606x.

So, I would like to send cast, unfinished sample parts, about 2" x 2", for some sort of plating/painting/anodizing process that closely matches the anodized treatment of the machined parts I will also send. It is an interior application. It can be a paint, a plating, or some combination, whatever works. Volumes up to 5K parts.

Cliff Hersh
Lighting OEM - Hayward, CA, USA
contact button


RFQ button

Dear Reader

Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com