Aluminium powder coated windows scratched
by other contractors
April 10, 2009
After completion of powder coating, we have fixed the aluminium
windows in the building walls, other contractors have scratched the
sections as well as powder coating, please tell what is the tolerance
in this as per standards.
Venkat Chalapathy