Wrinkle defect in galvanized steel sheet

May 12, 2009

Dear All ;

I am an metallurgical and materials engineer and working in sheet steel factory in Turkey.
As shown in the picture ; there is a wrinkle defect (mark) in our galvanized sheet steels and we do not know the root reason of this problem.

We have a continuous galvanizing lines and we could not find any problem about process parameters (tensions, atmosphere and furnace temperatures are normal). Could you have any idea about this surface problem.

Regard

Turgut Kirma
engineer - Bursa, Turkey
contact button


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com