April 29, 2009

Some one could let me know what dyes used in sulfuric acid csolution for Acid cu bath.
Thanks a lot

Woo Jerry
employee - Guangdong, China
  ^- Privately contact this inquirer -^
May 12, 2009

There are several known organic dyes, which can help to improve the levelling:

Janus Green B (Diethyl Safranine Azo Aniline), Safranine T, Janus Black R, Janus Blue B etc. They can be obtained from Sigma-Aldrich. In any case they must be of high quality.

But it's quite hard to formulate good acid cu additives, you also need MPS, DPS, UPS, a well balanced mixture of special surfactants (incl. block copolymers), etc.

In your case I would contact Raschig company, as they supply many of the needed specialties.

Good luck!

Martin Michel
- Berlin, Germany


May 13, 2009

I had never heard of dyes being used in a copper plating bath, Jerry. I thank Martin for alerting me that, apparently, the brighteners used in acid copper can be dyes.

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search