Normalized 1008 steel, post induction braze - blistering zinc chromate  

April 30, 2009

We're performing an induction 1008 steel braze with a copper ring in Nitrogen atmosphere for the past 2 years. We've recently elected to do a normalizing operation at 1600 deg. F for 10 minutes to relieve forming stress from an earlier operation, prior to sending these parts for a zinc trivalent electroplate per B633 T3.

Problem is we're getting seeing blistering around the heat affected zone that hasn't come up from previous years of production without the normalize. Any idea's?

Dale Thomas
Buyer - Burlington, ON, Canada
contact button


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com