Want no-function (except thickness) coating for steel pipeMay 1, 2009 Dear All, Deman DEMRI
May 27, 2009 When you say 2mm do you mean 1mm per side (1 on top and 1 on
bottom of the pipe or 2+2 which gives you a diameter change of
4mm? Johnathan Posey
May 27, 2009 If there is literally no requirement other than thickness and ease of application, have you considered tape? There are plenty of different varieties that offer 2mm thickness.
![]() |
|