I would like to finish my door levers in a Satin Bronze finish
#612. What would be the best way to do it?
George Delgado
- Marlboro, NJ, USA

May 1 , 2009
Hi, George. (You posted this as as an industrial rather than a
consumer need, but you provided no company info). So what do you mean
by "my"? :-)
Are you a homeowner with existing levers on two or three doors, or
are you a casting foundry with several hundred per day?.
But in either case, you need to send them to a plating shop if you
want a real Satin Bronze. I;m not familiar with this "#612"
specification -- where did you get this?