Hi Dear:
I'm production manager of a wpc company. we produce counter tops with
a base of 75% wood fiber and 25% pp, but our customers need these
products with HPL laminates but we have to treat our surface...what
is the best way to treat these products?
Best Regards
Farrokh Janani
production manager - Tehran, Iran

April 27, 2009
Hi, Farrokh. You are saying that these counter tops already have a
slick and shiny WPC lamination layer on them, and now you want to
adhere an HPL on top of that? I believe that contact cement is the
normal way of adhering HPL to an underlayment, but I'm not sure if
that will stick to the top of this WPC that you are manufacturing.
Regards,
|
|

Ted Mooney, P.E.
finishing.com