Seeking 2.5 mil Cu plating of 30 pcs. of 316SS aprox. 10"X12"x3/16"

January 29, 2009

We need to plate 30 pcs. of 316 SS to a thickness of .0025 with Copper. The copper then needs to have a flash coating of nickel. Each piece to be plated is curved in two dimension. Total dimensions are approx. 10"x24"x3/16", but only half the piece is to be plated. The rest of it will need to be masked. We are located in NYC but are willing to ship.

Nicholas Rivera
research lab - New York City, New York, USA
  ^- Privately contact this inquirer -^



----
Readers: This site is made available for camaraderie & technical info exchange by our supporting advertisers, and they will contact the inquirer privately regarding their commercial needs. Please offer comments on any technical issues, but not sourcing suggestions or testimonials. Thanks!


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search