Activating and sensatizing graphite for electroless copper without palladium  

January 28, 2009

Can we activate and sensatise graphite with something cheaper instead of Stannous and palladium chloride method.I am working on graphite contacts project.

Dave

Davinder singh
student - India
contact button


February 4, 2009

Graphite conducts electricity, so, it is theoretically platable by conventional galvanic (electrolytic) methods. It only requires good cleaning.

Guillermo Marrufo
Monterrey, NL, Mexico


February 7, 2009

The problem with graphite is that it is porous and soaks up the different solutions, thus it is a bitch to plate.

James Watts
- FL


February 15, 2009

Electrolyticaly plating graphite is difficult due to holding powder and passing current in all particals,Any solution to this problem

Dave

Davinder Singh
- Chandigarh, India


February 19, 2009

What if you tried soaking in silver nitrate, replacing paladium chloride.


Cair Shishani

aircraft maintenance - Abu Dhabi, UAE


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com