January 29, 2009
I am Osveh from Iran I studied polymer and I have been working in
powder coating for more than 6 years, nowadays I try to formulate
some hammertone finish powdercoating but all of my effort doesn't
work, if some body can help me or suggestion some texturing agent for
powdercoating , I can also try to help him or her if I can do
something
my system is 50/50 hybrid,
I tested cab powder with filler and without filler but I could not
get a big texture all of them is fine , could you suggest me any
other kind of texturing agent, also I tested powdermate508 tex from
the troy company but I think because of my resins and their
viscosity,I couldn't get the right response.
Osveh Amerian
employe - Tehran, Iran

January 29, 2009
CAB is the right route... but depends upon the grade - are you
including a flow additive?
Try without or very low %.
-
-
 |