51078

How to mask  

January 22, 2009

Hello, I will work with a etch process and all the specs talk about mask the number of series of the piece, but dont say how? What can I use to do that?

Fer Baca
employee - Texas
contact button


January 28, 2009

Hi, Fer. You haven't given us any details of what metal you are etching, and with what chemicals. There are plugs and caps, tapes, waxes, and other technologies available. But if you explain your situation to a supplier of masking materials like the site's supporting advertiser Maskcoat, I think they can help you select an appropriate masking technology for your situation. Good luck.

Regards,


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey


February 9, 2009

Thanks for you advice

the metal is inconel and the etch solucion will be HF and HNO3. I was reading about wetting agents to improve the etch and the rinse process, this agent really work?

Fer Baca
- Texas


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com