51068
Results and disposal of materials stripped
from.......
January 11, 2009
what are the various materials produced from the various types of
acid stripping, nitric, sulfuric, hydrochloric. etc.
I want to do it a safe as possible and not pollute.
is there a resource that I can be directed to, I know this is a large
question.
thanks
engineer, not chemist.
Jim Nelson
engineer - Lincoln, NE, USA

January 28, 2009
Jim
The various acids used for stripping (metals) will contain those
target materials once the process begins. The actual stripping
process will release gasses unique to the reaction. Your end solution
will likely be a hazardous waste (characteristic or listed).
If you have not yet started your process, contact a consultant or
hazardous waste disposal company.
If you have started your process, contact a consultant or hazardous
waste disposal company, particularly if you do not have someone
knowledgable of the regulatory requirements for this process.
Google search "hazardous waste generator + Nebraska"
Willie Alexander
- Colorado Springs, CO
-
-
 |