Can I redo Zinc plate chromate?
January 26, 2009
Can I replate a part thats already been plated
Steven Kentbuyer - Durham, England
^- Privately contact this inquirer -^
January 26, 2009
Usually, Steven. It is possible for the base metal to get too pitted from repeated plating to be replateable without polishing or special methods, or to have other issues, but in the majority of cases the parts can be relatively simply stripped and replated.
Regards,
|