Submerged hook for anode sheets ?

January 24, 2009

I am trying to use 3mm copper anodes sheets for a tiny acid copper plating bath. Due to the thinness of the anode there is no place to drill and tap in a conventional titanium anode hook. Instead, I've decided to use the hooks upside down. That is, drill and tap a copper bus bar and screw in an upside down titanium hook. The bottom of the hook will be immersed in the bath with a copper anode sheet hanging via a small hole. My question is how well will this perform in terms of electrical connectivity ?
Must I always bolt to anodes ?

I did some measurements of titanium hooks and noticed large voltage drops occurring at the copper/titanium interface, sometimes a 1V drop. Worst, is that this resistance can vary widely. For paralleled anode this may cause poor current balancing. This is half expected since titanium has 24x resistance of copper, and itaniums also forms an oxide layer in air. I'm curious how other people handle these issues or is it normally insignificant ?

Adam Seychell
product designer - Melbourne, Australia
  ^- Privately contact this inquirer -^
January 27, 2009

Titanium is a very poor conductor of electricity. I would use brass wire as hooks. Mask if you absolutely need to.

James Watts
- Navarre, Florida

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search