Our high school just finished building a new gym with a new galvanized metal corrugated roof. I want to have our team name painted on the roof but not sure how to do it. The letters will be about 25 feet tall with the total length about 80 feet. I can't find a painter who knows how to do it or anyone to tell give me a specification or method.

David Medcalf
Construction Manager - St. Helena, California, USA
  ^- Privately contact this inquirer -^
February 3, 2009

I can't tell by looking at the photo you submitted but I'll assume that roof is galvanized metal and it is not painted. If this is true, then I would suggest you try a military-spec paint and system. The system would generally be a 1- wash primer, 2- type high solid primer, then 3- topcoat. These mil-spec paints might withstand the environment better than others and give you the longevity you require. I would check with some of the top paint manufacturers and see if they agree. That's my 2 cents worth...........


Bob Utech
Brooklyn Park, Minnesota

 
Editor's note: 
Mr. Utech is
the author of -->


A Guide to High Performance Powder Coating
[link is to Amazon]


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search