I am looking to set up a 220 litre/ 55 gallon drum factory,
instead of painting the drums we want to zinc plate them.
Is there anybody doing this, can one seam-weld zinc plated sheet or
do we need to make up drum bodies and plate after welding?
How do I go about setting up a Zinc plant as I have no knowledge re
equipment and consumeables etc?
Drums destined for the fruit-pulp industry, is zinc coating toxic for
foodstuffs ?
Any advise or assistance will be greatly appreciated
Peter Krichel
Drum manufacturer - Johannesburg Gauteng South Africa

January 23, 2009
Hi, Peter. Zinc is not a food-safe metal. Sorry, but this idea is
not a promising one.