Cost cutting in powder coating finishing  

January 22, 2009

Can I do simple powder coating on one side and good finish on other side of sheet metal components for cost savings. how much will be the savings.

Ajitkumar Gangadharan
Manufacturing Professional - Hyderabad, Andhra Pradesh, INDIA
contact button


January 26, 2009

The simple answer is yes... with the proviso the thin side will not now be aesthetically as good and rusting may occur. Mileage... costings for normal film wts vs low film wts go to the Mileage calculator (click on image to the left). Input 75 microns and powder cost etc... then repeat using 30, 40 or 50 microns, then you will see the difference in costings

Terry Hickling
Martex Paints Ltd
  
Birmingham, UK


Dear Reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com