Black oxide on Tribaloy T400 [New Zealand]

January 21, 2009

hi, we currently black oxide a lot of parts that also have hard chrome on them, the black oxide does not effect the chrome and just wipes of, unfortunately the chrome is being replaced with tribaloy T400 (Co,Mo,Cr,Si) does anyone know if black oxide would have any detrimental effect on this coating.

Steven Salt
- Auckland, New Zealand
  ^- Privately contact this inquirer -^
January 23, 2009

My guess is that it would be minimal unless there is also iron or aluminum in low %.
Run a few scrap parts or test panels and find out. I assume that this is a thermal spray. It may be slightly porous if it is flame sprayed. Far less if plasma sprayed and nearly non existent in the high energy processes.

James Watts
- Navarre, Florida

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search