January 20, 2009

A alkaline zinc alloy with clear and yellow chromates are found to be flaking once they arrive in mexico (but not black chromate), but do not flake directly after plating. A wetter/inhibitor was added to the acid bath to help with the hydrogen release but did not work. Parts are only flaking on I/D...

Tim Wines
Quality Mgr - Madison Heights, Michigan
  ^- Privately contact this inquirer -^

ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search