Does black oxidizing change the thickness of a part?
September 24, 2008We recently just made some parts and send them out to be black oxidized. Will this coating change the thickness of the part? thanks
Ben Knightengineer - Birmingham, Alabama
^- Privately contact this inquirer -^
September 24, 2008
No, Ben, it won't. The thickness is measured in millionths of an inch rather than ten thousandths or thousandths.
Regards,
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |